CERTIFIED REFERENCE MATERIAL
SE21-211
unalloyed steel

Version: 002      Date of certification: 10.06.22      Sample form: Milling 0.200-1.400 mm
Analyte Unit Certified value Confidence
interval (95%)
No. of independent
repeated series
Measuring
method*
  C
S
N
  %
%
%
      0.1080
0.0007
0.0102
      0.0025
0.0001
0.0001
 4
4
3
1,2
2
3
* Measuring method
1: Combustion with coulometric detection
2: Combustion with IR-detection
3: Hot extraction with HC and IR detection