| Analyte | Unit | Certified value | Confidence interval (95%) |
No. of independent repeated series |
Measuring method* |
C |
% |
0.2035 |
0.0009 |
12 |
1 |
Cr |
% |
0.023 |
0.002 |
5 |
2 |
As |
% |
0.0060 |
0.0002 |
4 |
3 |
Sn |
% |
0.00178 |
0.00002 |
6 |
2 |
Zn |
% |
0.00053 |
0.00001 |
6 |
2 |
| * Measuring method | |
| 1: Combustion with coulometric detection |
2: Atomic absorption spectrometry |
| 3: Photometry |
4: Combustion with IR-detection |