| Analyte | Unit | Certified value | Confidence interval (95%) |
No. of independent repeated series |
Measuring method* |
C |
% |
0.1406 |
0.0003 |
3 |
1 |
| * Measuring method | |
| 1: Combustion with coulometric detection |
2: Combustion with IR-detection |
| 3: Hot extraction with HC and IR detection |
  |